Lithium battery horizontal ribbon and plow blade mixer with tungsten carbide coating applied by spraying.

Spray powder: Tungsten carbide powder (10 cobalt 4 chromium 86 tungsten carbide / 12 cobalt 88 tungsten carbide)

Spraying thickness: 0.2–0.3 mm

Spraying Process: Supersonic Flame

Pore sealing: Imported pore-sealing agent with excellent anti-corrosion performance.

Our company undertakes the following types of spray mixing machines:

Horizontal ribbon mixers, horizontal plow blade mixers, double-cone spiral mixers; high-speed lithium-ion battery mixers, planetary power mixers, dispersion-type mixers, paddle dryers, and other mixing, stirring, and dispersing equipment.