What this video shows

This clip follows our technician through the SX-120 plasma spray control cabinet during a factory setup and test run. The camera moves across the front panel while the operator adjusts each circuit: powder gas pressure, vibrator gas for the powder hopper, spraying voltage and current, and the cooling-water temperature readout.

The panel carries bilingual Chinese/English labels, which is how machines for export are built. Watching the values change as the operator turns each knob is a useful introduction to what a plasma spray controller actually manages - and to the checks we record before a system is packed for shipment.

What each control does

  • Spraying voltage / current: set the arc power that determines plasma enthalpy and how completely the powder melts
  • Powder gas control: carries powder from the feeder into the plasma jet; too much or too little shifts the particle trajectory and deposition rate
  • Vibrator gas: keeps the hopper powder flowing evenly so feed rate does not drift during a long run
  • Water temperature: monitors the closed-loop cooling circuit that protects the gun and the power supply
  • HMI and interlocks: the touch screen sequences start-up, purge and shutdown and trips the system on a cooling or gas fault

Why we record the setup

A plasma coating is only repeatable if the same parameter set can be reloaded every time. During commissioning we store a baseline recipe for the customer's powder and part, print it in the handover doc and use it as the reference for later troubleshooting. If coating quality changes months later, the first check is always whether the gas, current and cooling readings still match this baseline.

The SX-120 is supplied as a complete cell - control cabinet, powder feeder, spray gun, cooling unit and hose set - with parameter sheets and operator training. We also support on-site commissioning and sample trials before full production.

Frequently asked questions

What do the spraying voltage and current readings mean?

They set the arc power of the plasma torch. Higher power increases the plasma enthalpy and powder melting, but also heats the substrate more, so the value is chosen together with standoff and traverse speed.

Why is powder gas adjusted separately from the plasma gas?

Powder gas only transports powder into the jet. Keeping it independent lets the operator tune injection depth and deposition rate without disturbing the arc itself.

Why monitor cooling-water temperature?

The gun and power supply run on a closed-loop water circuit. A rising temperature or a flow fault is an early warning of nozzle or hose trouble, so the controller interlocks the system.

Is the control panel available in English?

Yes. Export machines are built with bilingual Chinese/English labels, and the HMI and parameter sheets are supplied in English.

Do you provide commissioning and training?

Yes. Every system is tested with a baseline recipe before shipment, and we provide parameter sheets, operator training and optional on-site commissioning.

Related Processing Videos

Демонстрация порошкового покрытия SX-6018 методом огненного распыла 6:50
Thermal Spray

Демонстрация порошкового покрытия SX-6018 методом огненного распыла

Практическая демонстрация распыления порошка пламенем SX-6018: оператор формирует ровное полимерное покрытие на круглой стальной заготовке, регулируя пламя, расстояние и движение на глаз.

Смотреть видео →
Внутреннее ЧПУ-обрабатывание деталей подающего устройства для порошка 4:07
Thermal Spray

Внутреннее ЧПУ-обрабатывание деталей подающего устройства для порошка

Центр ЧПУ для механической обработки, выполняющий резку и сверление компонентов порошковых податчиков в нашей собственной мастерской — производственные возможности, стоящие за нашими распылительными пистолетами, податчиками и запасными частями.

Смотреть видео →
Покрытие из карбида вольфрама методом HVOF на винтах 2:13
HVOF

Покрытие из карбида вольфрама методом HVOF на винтах

Горелка HVOF наносит карбид вольфрама на вращающийся вал винта, перемещаясь вдоль спирали так, чтобы расстояние и покрытие оставались равномерными по всем виткам.

Смотреть видео →