Автоматическая линия цинкового дугового напыления для баллонов с СУГ

What this video shows

An automatic zinc arc spraying cell installed at an LPG cylinder manufacturer's plant in Lebanon. The camera moves around the enclosed spray booth, the wire reel rack and the control cabinet, showing how the cylinder body is presented to the arc spray guns and how the cycle is driven from the PLC panel.

Zinc is fed as two wires that are melted by an electric arc and atomised onto the cylinder surface. On a production line the value is not the spray itself but the repeatability: every cylinder gets the same traverse, the same standoff and the same coating weight, shift after shift.

Line configuration

  • Spray system: high-output twin-wire arc spray guns with independent wire feed reels
  • Enclosure: closed spray booth with extraction and dust collection to contain zinc fume and overspray
  • Motion: cylinder rotation plus programmed gun traverse, with a stored recipe per cylinder size
  • Control: PLC cabinet with status lamps and interlocks for wire, air and extraction
  • Process chain: abrasive blast to a clean profile, zinc arc spray, then visual and thickness inspection

Why zinc on LPG cylinders

Zinc gives galvanic protection to the steel even if the coating is scratched, which is why cylinder makers use it for outdoor and humid service. Arc spraying applies it quickly at production rates without a bath, and coating weight is easy to control through wire feed speed and traverse speed.

We build complete automatic zinc and aluminium arc spray lines - guns, power sources, booths, turntables or transfer tracks, extraction and PLC control - and commission them on site with the customer's own parts. The same layout is used for wind-power flanges, steel structures and other large components needing long-life corrosion protection.

Frequently asked questions

Why zinc instead of paint for LPG cylinders?

Zinc provides galvanic (sacrificial) protection, so a scratch does not turn into under-film rust. It also stands up better to handling and outdoor storage.

Why is the spray booth enclosed?

Arc spraying zinc produces fume and overspray. An enclosed booth with extraction keeps the work area clean, protects operators and recovers overspray.

How is coating thickness controlled on an automatic line?

Wire feed speed, cylinder rotation and gun traverse are stored as a recipe in the PLC; thickness is then verified by gauge on sample cylinders from each batch.

Can the line handle different cylinder sizes?

Yes. Fixtures and recipes are changed per cylinder diameter and height, and the traverse limits are stored so changeover is repeatable.

Do you supply the whole line or only the spray equipment?

We can supply the complete turnkey line - arc spray system, booth, extraction, motion system and PLC control - and commission it at the customer plant.

Related Processing Videos

Демонстрация порошкового покрытия SX-6018 методом огненного распыла 6:50
Thermal Spray

Демонстрация порошкового покрытия SX-6018 методом огненного распыла

Практическая демонстрация распыления порошка пламенем SX-6018: оператор формирует ровное полимерное покрытие на круглой стальной заготовке, регулируя пламя, расстояние и движение на глаз.

Смотреть видео →
Настройка и тестирование системы плазменного напыления SX-120 4:26
Plasma Spray

Настройка и тестирование системы плазменного напыления SX-120

Крупный план обхода шкафа управления плазменным напылением SX-120 во время ввода в эксплуатацию: перед тестовым запуском устанавливаются порошковый газ, газ для вибратора, напряжение распыления, ток и температура охлаждающей воды.

Смотреть видео →
Внутреннее ЧПУ-обрабатывание деталей подающего устройства для порошка 4:07