Home / Industry Cases / Printing
Printing - Real projects showing how thermal spray coatings solved wear and corrosion problems.
Flexo anilox rolls coated with plasma chromium oxide last about ten times longer than hard chrome. We coat and repair anilox, corrugating, calender and corona rolls with full regrinding and re-engraving.