Processing Videos

Workshop footage of real coating jobs: HVOF, plasma and arc spraying, roll grinding, fixturing and finishing.

Plasma Spray Turntable System Delivered to an Italian Customer 2:41
Plasma Spray

Plasma Spray Turntable System Delivered to an Italian Customer

A multi-position turntable plasma spraying cell running at our Italian customer's facility - fixtures rotate through the spray zone so every part receives a uniform coating.

Watch video →
Factory Overview - Thermal Spray Equipment Manufacturing 3:45

Factory Overview - Thermal Spray Equipment Manufacturing

A walkthrough of our production facility: the machining, assembly and test areas where SX-series thermal spray systems, spray guns and peripheral equipment are built and commissioned.

Watch video →
SX-60 Plasma Spraying Non-Stick Coating on Cookware 1:07
Plasma Spray

SX-60 Plasma Spraying Non-Stick Coating on Cookware

The compact SX-60 plasma spray system applying a ceramic non-stick coating to a pan interior - an entry-level cell for cookware factories and coating service shops.

Watch video →
SX-LP60 Low-Pressure Cold Spray System in Operation 0:27

SX-LP60 Low-Pressure Cold Spray System in Operation

The SX-LP60 low-pressure cold spray system building up dense metal coatings with compressed air instead of a combustion flame - ideal for repair and conductive coatings on sensitive parts.

Watch video →
Robotic Spraying a Large Framed Mesh Workpiece 1:00
Plasma Spray

Robotic Spraying a Large Framed Mesh Workpiece

A six-axis robot guides the spray torch across a large framed mesh panel, keeping a constant standoff for an even ceramic coating over the entire surface.

Watch video →
24-Station Rotary Disc Spraying System 1:17
Plasma Spray

24-Station Rotary Disc Spraying System

A 24-station rotary indexing disc coating workpieces in continuous production - load, spray and unload in one cycle for high-throughput, consistent quality.

Watch video →
SX-5000 HVOF System Commissioning for a Canadian Customer 1:37
HVOF

SX-5000 HVOF System Commissioning for a Canadian Customer

On-site acceptance test of the SX-5000 gas HVOF system at a Canadian customer's plant - start-up, spray parameter tuning and coating verification before handover.

Watch video →
Thermal Spray Technology Introduction 21:06
Thermal Spray

Thermal Spray Technology Introduction

A general introduction to thermal spray technology - heat sources, spray processes, coating materials and typical industrial applications.

Watch video →
Single-Station Cookware Spraying 1:07
Non-Stick Coating

Single-Station Cookware Spraying

Spraying non-stick primer and top coats on cookware at a single enclosed station - a compact solution for small batches, samples and special sizes.

Watch video →
SX-600 Arc Spray Equipment Demonstration 2:08
Arc Spray

SX-600 Arc Spray Equipment Demonstration

The SX-600 twin-wire arc spray system in operation - high-deposition coatings of zinc, aluminum and anti-corrosion alloys.

Watch video →
Internal Bore Spraying with the SG-100 Gun 0:09
Plasma Spray

Internal Bore Spraying with the SG-100 Gun

Coating the inside diameter of a bore with our SG-100 internal spray gun - a hard-to-reach area that most spray shops cannot coat.

Watch video →
Guide Roll Coating on the Spray Line 2:06
Roll Coating

Guide Roll Coating on the Spray Line

Surface preparation and spray coating of steel guide rolls used in paper, film and packaging lines - filmed on our production floor.

Watch video →
Battery Electrode Calender Roll Coating 1:12
HVOF Coating

Battery Electrode Calender Roll Coating

Workshop footage of a calender roll coating job for lithium-battery electrode production: part set-up, tungsten carbide spraying and surface finishing.

Watch video →
HVOF Spraying of NiCr-CrC and NiCr Alloy Coatings 0:26
HVOF Coating

HVOF Spraying of NiCr-CrC and NiCr Alloy Coatings

Supersonic HVOF spraying of NiCr-CrC and NiCr alloy powders onto steel components - dense, hard coatings for combined wear and corrosion protection.

Watch video →
Arc Spraying a Paper Machine Dryer Cylinder 0:10
Roll Coating

Arc Spraying a Paper Machine Dryer Cylinder

Twin-wire arc spraying rebuilds the surface of a paper machine dryer cylinder - restoring diameter and improving release.

Watch video →