Tungsten Carbide Powder HVOF / Plasma Arc Spray Gun

Tungsten Carbide Powder HVOF / Plasma Arc Spray Gun

Tungsten Carbide Powder HVOF / Plasma Arc Spray Gun

This spray gun is designed for tungsten carbide (WC-Co, WC-CoCr) and chromium carbide (Cr3C2-NiCr) powders. A fuel–oxygen mixture is continuously combusted in a chamber; the hot gas expands through a converging-diverging Laval nozzle and exits the barrel at supersonic speed, accelerating powder particles to about 800 m/s before they strike the substrate.

Coating performance

  • Porosity: <1%
  • Bond strength: up to 90 MPa
  • Coating hardness: approx. HV 1,450
  • Flame velocity: >2,000 m/s class; particle velocity up to 800 m/s

Spray materials

  • WC-Co, WC-CoCr (wear and abrasion resistance)
  • Cr3C2-NiCr (high-temperature wear resistance)
  • MCrAlY bond coats, self-fluxing alloys

Typical applications

  • Screw and barrel wear protection in plastic machinery
  • Corrugated roll coating and repair
  • Pump shafts, valves, and hydraulic rods
  • Paper mill dryer cylinders and fans