One Coating, Three Kinds of Protection
Fine tungsten carbide particles sprayed onto metal surfaces form a hard, dense layer that simultaneously improves wear resistance, corrosion resistance and high-temperature stability - a proven answer for expensive components in aggressive duty.
Key Properties
- Hardness up to HRC 85-92, far above most metallic materials
- Withstands severe friction, abrasion and particle erosion
- Resistant to a wide range of acids, alkalis and salts
- Stable at temperatures up to 1000 C
- Flexible application by plasma, flame or arc spraying
Industries and Parts
- Aerospace: engine blades, turbine rotors
- Automotive: valve seat inserts, piston rings, crankshaft bearings
- Oil and gas: drilling tools, pump bodies, valves
- Power: boiler tubes, steam piping, turbine blades
- Chemical: reactors, heat exchangers, agitators
- Metallurgy: continuous casting rolls, working rolls, dies
Process Control
Automated parameter control delivers uniform, dense coatings; powder quality and spraying distance are tightly managed to guarantee repeatable performance part after part.