SX-1000 High-Power Intelligent Arc Spray System

SX-1000 High-Power Intelligent Arc Spray System

The SX-1000 is a high-power, intelligent arc spray system built for batch production and large-area anti-corrosion work. A 36 kW / 1000 A flat-characteristic power supply melts wires more completely than smaller units, while a Siemens PLC and industrial touch screen provide closed-loop control of voltage, current, air pressure and wire feed. Optional robot integration turns the SX-1000 into a fully automatic coating cell.

Key Specifications

  • Power: 36 kW / 1000 A
  • Wire diameter: 1.2 – 3.0 mm
  • Air consumption: 4.6 m³/min
  • Typical spray rates: Zn 46 kg/h, Al 20 kg/h, Cu 41 kg/h, carbon steel 43.5 kg/h, stainless steel 43.5 kg/h
  • Control: Siemens touch screen + PLC with data logging and fault alarm
  • Gun options: push/pull feed, including imported atomizing gun
  • Automation ready: 6-axis robot + AGV + rotary table integration

التطبيقات

  • Large-area zinc/aluminum anti-corrosion for bridges, towers and steel structures
  • Batch processing of pre-stressed anchors, transition pipes and flanges
  • Automatic production lines with robot, rotary table and dust collection
  • Repair and protection of shafts, cylinders and large rotating parts