The SX-9000 is a kerosene-fueled high-velocity oxygen-fuel (HVOF) spray system. Kerosene is atomized with oxygen, ignited in a combustion chamber, and accelerated through a Laval nozzle to produce a supersonic flame stream. Powder is injected radially into the flame, heated and accelerated to high velocity before impacting the workpiece, forming extremely dense, high-bond-strength coatings.
Key Specifications
- Flame speed: ~2100 m/s
- Flame temperature: ~5000 °C
- Equivalent gun power: 150 kW
- Particle velocity: 1100 m/s
- Coating porosity: <1%
- Coating bond strength: >90 MPa
- Suitable powder size: 10 – 45 μm
- Gun weight: ~4.5 kg
- Control: Siemens PLC + touch screen; SMC and Omron components
Aplicaciones
- Tungsten carbide, chromium carbide and metal-ceramic coatings
- Pump shafts, piston rods, plungers, valves and gates
- Industrial rolls, paper-machine rolls and calender rolls
- Aerospace, power generation, petroleum, mining and paper industries