Thermal Spray Materials (Powders & Wires)
Thermal spray powders and wires: tungsten carbide, chromium oxide, zirconia, yttria, NiCr-Cr3C2, titania and magnesia powder plus arc spray wire.

Thermal Spray Wire Series (Arc Spray)
Arc spray wire in zinc, aluminium, zinc-aluminium, copper, stainless, nickel-aluminium and molybdenum - 1.6 to 3.0 mm, for corrosion protection, dimensional restoration and conductive layers.
Read more →
Spherical Magnesium Oxide Powder
Spheroidised magnesia powder for high-temperature insulation, plasma-resistant coatings and spheroidisation feedstock - 2852 C melting point with excellent flow for consistent feeding.
Read more →
Titanium & Titanium Oxide Powder
Titanium, titanium dioxide and titanium sub-oxide powders for biomedical bond layers, corrosion resistant coatings, conductive electrodes and photocatalytic surfaces.
Read more →
Nickel Chrome Chromium Carbide Powder
NiCr-Cr3C2 powder for coatings that hold their wear resistance at 800-900 C - the standard choice where tungsten carbide would oxidise, such as boiler tubes, high temperature valves and turbine components.
Read more →
Yttria Powder (Y2O3)
High-purity yttrium oxide powder for plasma-sprayed coatings in semiconductor, crucible and high-temperature service - 2425 C melting point, excellent plasma erosion resistance and low contamination.
Read more →
Zirconia Powder (YSZ / Calcia Stabilised)
Zirconia powders for thermal barrier and wear coatings - yttria-stabilised, calcia-stabilised and magnesia-stabilised grades, with the phase stability and porosity that decide whether a TBC survives thermal cycling.
Read more →
Chromium Oxide Powder (Cr2O3)
Chromium oxide powder for plasma-sprayed wear and corrosion resistant ceramic coatings - hard, chemically inert and electrically insulating, the standard choice for pump seals, sleeves and textile machinery.
Read more →
Tungsten Carbide Powder (WC-Co / WC-CoCr)
Composite tungsten carbide powders for HVOF and plasma spraying - WC-Co, WC-CoCr and WC-Ni grades with the cobalt content, particle size and morphology that decide hardness, toughness and corrosion resistance.
Read more →