المعالجة بالرش بالبلازما
المعالجة بالرش بالبلازما

Graphite Boat Zirconia (Yttria-Stabilized) Coating Service
Plasma-sprayed yttria-stabilized zirconia (YSZ) coating for graphite boat dishes, crucibles and plates used in cemented carbide sintering. Processed on SX-80 plasma spray systems with imported SG-100 guns, delivering high-temperature corrosion resistance and extended service life.
اقرأ المزيد
Plasma Spraying Ceramic Coating Process
A plasma torch ionises argon or nitrogen into a high-temperature jet that melts ceramic powder and propels it onto the workpiece. The coating gives the part hardness, wear resistance, heat resistance, corrosion resistance, insulation and thermal insulation in one process.
اقرأ المزيد
HVOF Tungsten Carbide Coating for Pump Shafts and Piston Rods
Pump shafts, piston rods and plungers carry seals and packings against a running surface, so wear there leads directly to leakage. A HVOF tungsten carbide coating gives that surface a dense, hard and corrosion-resistant layer that keeps the seal interface in good condition.
اقرأ المزيد
Arc Spray Coating for Large Wheels, Discs and Rotating Parts
Large wheels, discs, sheaves and rolls are expensive to replace and often impossible to source quickly. Arc spraying rebuilds their worn working surfaces and can add a wear or corrosion resistant layer at the same time, typically at a fraction of replacement cost.
اقرأ المزيد
Anti-Corrosion Surface Treatment for Steel Structures and Steelwork
For structural steel that has to survive decades of humid, coastal or chemical exposure, a thermally sprayed metal coating outperforms paint systems on its own. The sprayed layer protects the steel by sacrificial action, and the paint topcoat then only has to protect the coating itself.
اقرأ المزيد
On-Site Pipeline Thermal Spray Coating and Field Repair
Many pipelines and large steel components cannot be moved to a coating workshop. Our mobile crews prepare the surface and apply the coating on location, restoring corrosion protection or wear resistance with minimal disruption to production.
اقرأ المزيد
Zinc-Aluminum Arc Spray Anti-Corrosion Coating for Tanks and Vessels
Twin wire arc spraying of zinc-aluminum deposits a metallurgically bonded, sacrificial coating on steel surfaces. The zinc-aluminum layer corrodes preferentially and protects the steel underneath, which makes it a durable and economical answer for large steel surfaces in industrial and marine atmospheres.
اقرأ المزيد
Chrome Oxide Ceramic Coating for Sleeves and Bushings
Chrome oxide ceramic coating gives sleeves and bushings a hard, smooth and chemically stable working surface. It is the standard choice where the part must resist abrasive wear and mild corrosion at the same time, and where a low-friction running surface against a shaft or seal is essential.
اقرأ المزيد
Rolls and Shafts Plasma Spray Coating for Dimensional Restoration
When a roll or shaft is worn undersize, scored or corroded, plasma spray coating rebuilds it back to drawing tolerance instead of scrapping the part. We spray a ceramic, carbide or metal alloy layer, then grind and polish to the required diameter, hardness and surface finish.
اقرأ المزيد
Fan and Blower Impeller Wear-Resistant Coating for Dust-Laden Air
Induced draft and process fans that move dust-laden gas lose their blades to erosion within months. Coating the impeller blades and inlet cone with a carbide or ceramic layer raises the erosion resistance of the working surfaces, so the fan holds its balance and air flow for far longer.
اقرأ المزيد
Pump Impeller Tungsten Carbide Coating for Slurry and Seawater Pumps
Impeller erosion is one of the most common causes of pump failure in slurry, dredging and seawater service. Our tungsten carbide coating rebuilds and protects the impeller flow passages and vane edges, restoring hydraulic performance while sharply reducing the erosion rate.
اقرأ المزيد
Mixer Blade Tungsten Carbide Coating for Abrasive Mixing Duty
Mixer blades and agitator paddles wear out fast when they run in abrasive slurries, powders or corrosive chemical media. We apply a dense HVOF tungsten carbide coating to the blade surface, giving the part a hard, well-bonded wear layer that keeps the mixing profile intact far longer than an uncoated blade.
اقرأ المزيد
Nickel-Aluminium Coating for Hydrogen Production Electrode Mesh
Using Atmospheric Plasma Spraying (APS) technology, high-purity nickel (Ni) and aluminum (Al) composite powders are melted in a high-temperature plasma flame and sprayed onto the surface of a three-dimensional porous nickel mesh at high speed to form a micro-nano structure composite coating.
اقرأ المزيد
Plasma Cladding and Nano Ceramic Coating for Acid, Alkali and High-Temperature Wear
Guangzhou Sanxin/Zhuzhou Sanxin Metal Technology uses plasma spraying (APS) technology to prepare dense, high-bonding ceramic coatings on the internal/external surfaces of the equipment to achieve an economical and efficient protection solution of "coating instead of lining, coating instead of mater
اقرأ المزيد
Plasma Cladding and Nano Ceramic Coatings for Lithium Battery Plant Equipment
Guangzhou Sanxin provides professional equipment construction services for the lithium battery industry, covering plasma cladding coating and nano-ceramic coating technology. These advanced surface treatment technologies can significantly improve the performance and life of lithium battery equipment
اقرأ المزيد
High Wear-Resistant Ceramic Coating for Lithium Battery Material Crushers
New energy lithium battery equipment is specially designed for the lithium battery industry, providing efficient and reliable material transportation and mixing solutions. This series of equipment integrates advanced mechanical design and precision manufacturing technology and is suitable for the pr
اقرأ المزيد