Coating Services

Coating services for wear, corrosion and high temperature on rolls, shafts, pumps, dies and graphite parts.

Rolls and Shafts Plasma Spray Coating for Dimensional Restoration
Plasma Spraying Processing

Rolls and Shafts Plasma Spray Coating for Dimensional Restoration

When a roll or shaft is worn undersize, scored or corroded, plasma spray coating rebuilds it back to drawing tolerance instead of scrapping the part. We spray a ceramic, carbide or metal alloy layer, then grind and polish to the required diameter, hardness and surface finish.

Read more →
Fan and Blower Impeller Wear-Resistant Coating for Dust-Laden Air
Plasma Spraying Processing

Fan and Blower Impeller Wear-Resistant Coating for Dust-Laden Air

Induced draft and process fans that move dust-laden gas lose their blades to erosion within months. Coating the impeller blades and inlet cone with a carbide or ceramic layer raises the erosion resistance of the working surfaces, so the fan holds its balance and air flow for far longer.

Read more →
Pump Impeller Tungsten Carbide Coating for Slurry and Seawater Pumps
Plasma Spraying Processing

Pump Impeller Tungsten Carbide Coating for Slurry and Seawater Pumps

Impeller erosion is one of the most common causes of pump failure in slurry, dredging and seawater service. Our tungsten carbide coating rebuilds and protects the impeller flow passages and vane edges, restoring hydraulic performance while sharply reducing the erosion rate.

Read more →
Mixer Blade Tungsten Carbide Coating for Abrasive Mixing Duty
Plasma Spraying Processing

Mixer Blade Tungsten Carbide Coating for Abrasive Mixing Duty

Mixer blades and agitator paddles wear out fast when they run in abrasive slurries, powders or corrosive chemical media. We apply a dense HVOF tungsten carbide coating to the blade surface, giving the part a hard, well-bonded wear layer that keeps the mixing profile intact far longer than an uncoated blade.

Read more →
Nickel-Aluminium Coating for Hydrogen Production Electrode Mesh
Plasma Spraying Processing

Nickel-Aluminium Coating for Hydrogen Production Electrode Mesh

Using Atmospheric Plasma Spraying (APS) technology, high-purity nickel (Ni) and aluminum (Al) composite powders are melted in a high-temperature plasma flame and sprayed onto the surface of a three-dimensional porous nickel mesh at high speed to form a micro-nano structure composite coating.

Read more →
Plasma Cladding and Nano Ceramic Coating for Acid, Alkali and High-Temperature Wear
Plasma Spraying Processing

Plasma Cladding and Nano Ceramic Coating for Acid, Alkali and High-Temperature Wear

Guangzhou Sanxin/Zhuzhou Sanxin Metal Technology uses plasma spraying (APS) technology to prepare dense, high-bonding ceramic coatings on the internal/external surfaces of the equipment to achieve an economical and efficient protection solution of "coating instead of lining, coating instead of mater

Read more →
Plasma Cladding and Nano Ceramic Coatings for Lithium Battery Plant Equipment
Plasma Spraying Processing

Plasma Cladding and Nano Ceramic Coatings for Lithium Battery Plant Equipment

Guangzhou Sanxin provides professional equipment construction services for the lithium battery industry, covering plasma cladding coating and nano-ceramic coating technology. These advanced surface treatment technologies can significantly improve the performance and life of lithium battery equipment

Read more →
High Wear-Resistant Ceramic Coating for Lithium Battery Material Crushers
Plasma Spraying Processing

High Wear-Resistant Ceramic Coating for Lithium Battery Material Crushers

New energy lithium battery equipment is specially designed for the lithium battery industry, providing efficient and reliable material transportation and mixing solutions. This series of equipment integrates advanced mechanical design and precision manufacturing technology and is suitable for the pr

Read more →
Arc Spray Shaft Wear Repair Service for Motor Shafts, Crusher Shafts and Rotors
Plasma Spraying Processing

Arc Spray Shaft Wear Repair Service for Motor Shafts, Crusher Shafts and Rotors

One-stop on-site restoration of worn motor shafts, crusher transmission shafts and rotors using arc spraying, electric brush plating, laser cladding and cold welding. Original dimensions and performance restored at up to 70 percent below replacement cost.

Read more →
Plasma Sprayed Chromium Oxide (Cr2O3) Insulating Ceramic Coating Service
Coating Services

Plasma Sprayed Chromium Oxide (Cr2O3) Insulating Ceramic Coating Service

High-purity chromium oxide coatings applied by plasma spraying for dense, uniform electrically insulating layers on metal parts. Stable above 1000 C, hardness 1200-1400 HV, excellent chemical stability for power, electronics and petrochemical equipment.

Read more →
Tungsten Carbide Coating for Water Pumps, Slurry Pumps and Sewage Pumps
Coating Services

Tungsten Carbide Coating for Water Pumps, Slurry Pumps and Sewage Pumps

Thermal sprayed tungsten carbide coatings for impellers, pump casings, shaft sleeves and seals. Hardness 1500-1800 HV with strong corrosion resistance dramatically extends pump service life in abrasive and corrosive duty.

Read more →
Supersonic Arc Spray Coating for Converter Hoods and Flue Ducts
Plasma Spraying Processing

Supersonic Arc Spray Coating for Converter Hoods and Flue Ducts

A three-layer composite supersonic arc sprayed coating for converter hoods, flue ducts and power boiler water walls. Proven in service to extend life beyond three years against sulfur corrosion, high-temperature oxidation and erosion.

Read more →
Lithium Battery Equipment Coating Service - Plasma Cladding and Nano Ceramic Coatings
Coating Services

Lithium Battery Equipment Coating Service - Plasma Cladding and Nano Ceramic Coatings

Plasma cladding and nano ceramic coating services for lithium battery manufacturing equipment. Higher hardness, corrosion resistance, insulation and oxidation stability for battery casings, current collectors, electrodes and seals.

Read more →
Thermal Spray Tungsten Carbide Coatings - Wear, Corrosion and High-Temperature Protection
Coating Services

Thermal Spray Tungsten Carbide Coatings - Wear, Corrosion and High-Temperature Protection

Tungsten carbide (WC) thermal spray coatings for metal parts in aerospace, automotive, oil and gas and power generation. Hardness up to HRC 85-92, stable at 1000 C, applied by plasma, flame or arc spray.

Read more →
Plasma Sprayed Yttria-Stabilized Zirconia (YSZ) Thermal Barrier Coatings for Aero Engine Components
Plasma Spraying Processing

Plasma Sprayed Yttria-Stabilized Zirconia (YSZ) Thermal Barrier Coatings for Aero Engine Components

YSZ thermal barrier coatings for turbine and nozzle blades raise surface temperature capability above 1200 C while lowering base metal temperature by 300-500 C. MCrAlY bond coats, HVOF WC-Co for compressor blades.

Read more →