Coating Services

Coating services for wear, corrosion and high temperature on rolls, shafts, pumps, dies and graphite parts.

SX-80 Plasma Spraying System and Plasma Spheroidization Powder Production Equipment
Plasma Spheroidization Powder Production

SX-80 Plasma Spraying System and Plasma Spheroidization Powder Production Equipment

SX-80 high-energy plasma spraying system, 80-120 kW, with PLC control and SG-100 gun, for ceramic coating production and plasma spheroidization powder manufacturing. Complete line with powder feeding, cooling and classifying options.

Read more →
Plasma Sprayed Ceramic Wear-Resistant and Insulating Coatings
Insulating Coating Spraying Equipment

Plasma Sprayed Ceramic Wear-Resistant and Insulating Coatings

Contract plasma spraying service with alumina, chromia, zirconia and AT ceramic powders. Dense wear-resistant and insulating coatings with porosity below 1 percent and bond strength above 70 MPa, for parts of any size.

Read more →
Ceramic Coating for Plungers - Wear-Resistant and Insulating Special Ceramic Parts
Insulating Coating Spraying Equipment

Ceramic Coating for Plungers - Wear-Resistant and Insulating Special Ceramic Parts

Plasma sprayed special ceramic coating for pump plungers, pistons and special ceramic components. Dense, hard and electrically insulating coating with a ground and polished finish for long service life in abrasive, corrosive duty.

Read more →
HVOF and Plasma Ceramic Insulating Coating for Printing Machine Rollers
Insulating Coating Spraying Equipment

HVOF and Plasma Ceramic Insulating Coating for Printing Machine Rollers

Wear-resistant, insulating and high-temperature resistant ceramic coating for printing machine rubber rollers and corona rollers, applied by HVOF and plasma processes. Worn rollers can be stripped, re-coated and precision ground back to size.

Read more →
Ceramic Insulating Coating for Corona Rollers
Insulating Coating Spraying Equipment

Ceramic Insulating Coating for Corona Rollers

High-energy plasma sprayed alumina ceramic insulating coating for corona rollers on film treatment lines. Bond strength above 65 MPa, microhardness about HV0.3 780, thickness 0.5-2.0 mm, no breakdown at 10-20 kV / 10-30 kHz.

Read more →
Graphite Boat Zirconia (Yttria-Stabilized) Coating Service
Plasma Spraying Processing

Graphite Boat Zirconia (Yttria-Stabilized) Coating Service

Plasma-sprayed yttria-stabilized zirconia (YSZ) coating for graphite boat dishes, crucibles and plates used in cemented carbide sintering. Processed on SX-80 plasma spray systems with imported SG-100 guns, delivering high-temperature corrosion resistance and extended service life.

Read more →
Alumina and Plasma Spraying Equipment (SX-80 System)
Plasma Spray Equipment

Alumina and Plasma Spraying Equipment (SX-80 System)

The SX-80 plasma spraying system pairs an imported SG-100 plasma torch with an intelligent PLC control system for alumina and ceramic coating work. 100 kW class multi-mode operation, internal or external powder feeding, and components that last up to three times longer.

Read more →
Insulating and Shielding Coating for Coating Machines
Electronics and Semiconductor Industry

Insulating and Shielding Coating for Coating Machines

Alumina ceramic insulating and shielding coatings for electronic-industry coating machines, spray-fused with American Miller plasma equipment. Alumina purity above 99%, dielectric withstand 4000 V, uniform 50 um thickness, 15 MPa adhesion and HV900 hardness.

Read more →
Plasma Spraying Ceramic Coating Process
Plasma Spraying Processing

Plasma Spraying Ceramic Coating Process

A plasma torch ionises argon or nitrogen into a high-temperature jet that melts ceramic powder and propels it onto the workpiece. The coating gives the part hardness, wear resistance, heat resistance, corrosion resistance, insulation and thermal insulation in one process.

Read more →
HVOF Tungsten Carbide Coating for Pump Shafts and Piston Rods
Plasma Spraying Processing

HVOF Tungsten Carbide Coating for Pump Shafts and Piston Rods

Pump shafts, piston rods and plungers carry seals and packings against a running surface, so wear there leads directly to leakage. A HVOF tungsten carbide coating gives that surface a dense, hard and corrosion-resistant layer that keeps the seal interface in good condition.

Read more →
Arc Spray Coating for Large Wheels, Discs and Rotating Parts
Plasma Spraying Processing

Arc Spray Coating for Large Wheels, Discs and Rotating Parts

Large wheels, discs, sheaves and rolls are expensive to replace and often impossible to source quickly. Arc spraying rebuilds their worn working surfaces and can add a wear or corrosion resistant layer at the same time, typically at a fraction of replacement cost.

Read more →
Anti-Corrosion Surface Treatment for Steel Structures and Steelwork
Plasma Spraying Processing

Anti-Corrosion Surface Treatment for Steel Structures and Steelwork

For structural steel that has to survive decades of humid, coastal or chemical exposure, a thermally sprayed metal coating outperforms paint systems on its own. The sprayed layer protects the steel by sacrificial action, and the paint topcoat then only has to protect the coating itself.

Read more →
On-Site Pipeline Thermal Spray Coating and Field Repair
Plasma Spraying Processing

On-Site Pipeline Thermal Spray Coating and Field Repair

Many pipelines and large steel components cannot be moved to a coating workshop. Our mobile crews prepare the surface and apply the coating on location, restoring corrosion protection or wear resistance with minimal disruption to production.

Read more →
Zinc-Aluminum Arc Spray Anti-Corrosion Coating for Tanks and Vessels
Plasma Spraying Processing

Zinc-Aluminum Arc Spray Anti-Corrosion Coating for Tanks and Vessels

Twin wire arc spraying of zinc-aluminum deposits a metallurgically bonded, sacrificial coating on steel surfaces. The zinc-aluminum layer corrodes preferentially and protects the steel underneath, which makes it a durable and economical answer for large steel surfaces in industrial and marine atmospheres.

Read more →
Chrome Oxide Ceramic Coating for Sleeves and Bushings
Plasma Spraying Processing

Chrome Oxide Ceramic Coating for Sleeves and Bushings

Chrome oxide ceramic coating gives sleeves and bushings a hard, smooth and chemically stable working surface. It is the standard choice where the part must resist abrasive wear and mild corrosion at the same time, and where a low-friction running surface against a shaft or seal is essential.

Read more →